Acrylic are bonded in extremely humid conditions
When substrate loses moisture after installation
Debonding in certain areas because of uneven substrate surface
Insufficient or lack of pressing during the bonding period of laminate
Use Of extremely large acrylic/PVC laminate sheets (more than 8 ft x 2 ft long)
Use of water base synthetic resin adhesive any other the PEVA
Parameters | Ozone Acrylic Laminate | High Gloss Laminate Mica | PU Coating / Duco Paint | Back Painted Glass |
---|---|---|---|---|
Gloss Level | >90 | >70 | >85 | >85 |
Scratch Proof | 6H ANTI SCRATCH | No | No | No |
Color Consistency | Excellent | Not Good | Not Good | Not Good |
Orange peel | No | Yes | Yes | No |
UV Resistance | Excellent | Bad | Bad | Bad |
Water Resistance | Excellent | Bad | Bad | Excellent |
DRY Heat Resistance | Excellent | Good | Bad | Bad |
Volatile Organic Compounds (VOCs) | No | Yes | Yes | Yes |